W Schiffchen TF20112-20-4830
- Plansee Materialnummer
- 11372303
- Plansee Materialnummer
- 11372303
- Material
- W
- Stärke
- 0.2 mm, 0.0079 inch
- Breite
- 20 mm, 0.7874 inch
- Länge
- 112 mm, 4.4094 inch
- Höhe
- 7 mm, 0.2756 inch
- Wannenlänge
- 48 mm, 1.8898 inch
- Tiefe
- 3 mm, 0.1181 inch
- Füllvolumen
- 1.8 mm, 0.0709 inch
No documents available for this product.