W Schiffchen TF25112-20-8090

undefined
Plansee Materialnummer
11372307
STK
Plansee Materialnummer
11372307
Material
W
Stärke
0.2 mm, 0.0079 inch
Breite
25 mm, 0.9843 inch
Länge
112 mm, 4.4094 inch
Höhe
19 mm, 0.748 inch
Wannenlänge
80 mm, 3.1496 inch
Tiefe
9 mm, 0.3543 inch
Füllvolumen
11.53 mm, 0.4539 inch