W Schiffchen TF15100-30-4024
- Plansee Materialnummer
- 11372311
- Plansee Materialnummer
- 11372311
- Material
- W
- Stärke
- 0.3 mm, 0.0118 inch
- Breite
- 15 mm, 0.5906 inch
- Länge
- 100 mm, 3.937 inch
- Höhe
- 8 mm, 0.315 inch
- Wannenlänge
- 40 mm, 1.5748 inch
- Tiefe
- 2.4 mm, 0.0945 inch
- Füllvolumen
- 0.75 mm, 0.0295 inch
No documents available for this product.