W Schiffchen TO16100-30-3429

undefined
Plansee Materialnummer
11386682
STK
Plansee Materialnummer
11386682
Material
W
Stärke
0.3 mm, 0.0118 inch
Breite
16 mm, 0.6299 inch
Länge
100 mm, 3.937 inch
Höhe
7 mm, 0.2756 inch
Wannenlänge
34 mm, 1.3386 inch
Tiefe
2.9 mm, 0.1142 inch
Füllvolumen
0.61 mm, 0.024 inch