W Schiffchen TF15102-20-4025

undefined
Plansee Materialnummer
11501152
STK
Plansee Materialnummer
11501152
Material
W
Stärke
0.2 mm, 0.0079 inch
Breite
15 mm, 0.5906 inch
Länge
102 mm, 4.0157 inch
Höhe
10 mm, 0.3937 inch
Wannenlänge
40 mm, 1.5748 inch
Tiefe
2.5 mm, 0.0984 inch
Füllvolumen
0.84 mm, 0.0331 inch