W Schiffchen TS25075-30-2430

undefined
Plansee Materialnummer
11739522
STK
Plansee Materialnummer
11739522
Material
W
Stärke
0.3 mm, 0.0118 inch
Breite
25 mm, 0.9843 inch
Länge
75 mm, 2.9528 inch
Höhe
7 mm, 0.2756 inch
Wannenlänge
24 mm, 0.9449 inch
Tiefe
3 mm, 0.1181 inch
Füllvolumen
0.62 mm, 0.0244 inch

No documents available for this product.