W boat TF15100-30-4024

undefined
Plansee Material Number
11372311
PCE
Plansee Material Number
11372311
Material
W
Thickness
0.3 mm, 0.0118 inch
Width
15 mm, 0.5906 inch
Length
100 mm, 3.937 inch
Height
8 mm, 0.315 inch
Length of tub
40 mm, 1.5748 inch
Depth
2.4 mm, 0.0945 inch
Filling volume
0.75 mm, 0.0295 inch

No documents available for this product.