Mo boat SF08100-50-4020

undefined
Plansee Material Number
11416390
PCE
Plansee Material Number
11416390
Material
MO
Thickness
0.5 mm, 0.0197 inch
Width
8 mm, 0.315 inch
Length
100 mm, 3.937 inch
Height
1.7 mm, 0.0669 inch
Length of tub
40 mm, 1.5748 inch
Depth
2 mm, 0.0787 inch
Filling volume
0.27 mm, 0.0106 inch