Rods
TZM rod Ø 10,0 mm, ground
Contact
TZM rod Ø 10,0 mm, ground
Expand image
Plansee Material Number
22530
Quantity
M
Add to cart
Request for quote
Specifications
Plansee Material Number
22530
Material
TZM
Diameter
10 mm, 0.3937 inch
Length
0 mm, 0 inch
Documents