Mo boat bottom NB17100-15-4075
- Plansee Material Number
- 11371173
- Plansee Material Number
- 11371173
- Material
- MO
- Thickness
- 0.15 mm, 0.0059 inch
- Width
- 17 mm, 0.6693 inch
- Length
- 100 mm, 3.937 inch
- Height
- 8 mm, 0.315 inch
- Length of tub
- 40 mm, 1.5748 inch
- Depth
- 7.5 mm, 0.2953 inch
- Filling volume
- 4.32 mm, 0.1701 inch
No documents available for this product.