Mo Sheet 8 x 520 x 1300 mm
- Plansee Material Number
- 14473190
- Plansee Material Number
- 14473190
- Material
- MO
- Thickness
- 8 mm, 0.315 inch
- Width
- 520 mm, 20.4724 inch
- Length
- 1300 mm, 51.1811 inch
- Total cutting length
- 3640 mm, 143.3071 inch
- No. start holes
- 1 mm, 0.0394 inch