W Sheet 0,127 x 508 x 838,2 mm

undefined
Plansee Material Number
15267453
PCE
Plansee Material Number
15267453
Material
W
Thickness
0.127 mm, 0.005 inch
Width
508 mm, 20 inch
Length
838.2 mm, 33 inch
Rolled width
0 mm, 0 inch
Rolled length
0 mm, 0 inch
Thickness tolerance +
0 mm, 0 inch
Thickness tolerance –
0 mm, 0 inch