Mo sheet .015" x 24" x min. 372.05"

undefined
Plansee Material Number
11039184
PCE
Plansee Material Number
11039184
Material
MO
Thickness
0.381 mm, 0.015 inch
Width
609.6 mm, 24 inch
Length
10500 mm, 413.3858 inch
Rolled width
0 mm, 0 inch
Rolled length
0 mm, 0 inch
Thickness tolerance +
0.02 mm, 8.0E-4 inch
Thickness tolerance –
0.02 mm, 8.0E-4 inch