SPARKAL®X rod Dia 1,38" X 13,78"

undefined
Plansee Material Number
11191953
PCE
Plansee Material Number
11191953
Material
SPX
Width
0 mm, 0 inch
Length
350 mm, 13.7795 inch
Thickness
0 mm, 0 inch
Diameter
35 mm, 1.378 inch
Inner diameter
0 mm, 0 inch
Outside diameter
0 mm, 0 inch