Mo boat SF10100-30-5021

undefined
Plansee Material Number
11371010
PCE
Plansee Material Number
11371010
Material
MO
Thickness
0.3 mm, 0.0118 inch
Width
10 mm, 0.3937 inch
Length
100 mm, 3.937 inch
Height
2.1 mm, 0.0827 inch
Length of tub
50 mm, 1.9685 inch
Depth
2.1 mm, 0.0827 inch
Filling volume
0.54 mm, 0.0213 inch