Mo boat set NB25100-15-4015

undefined
Plansee Material Number
11371238
PCE
Plansee Material Number
11371238
Material
MO
Thickness
0.15 mm, 0.0059 inch
Width
25 mm, 0.9843 inch
Length
100 mm, 3.937 inch
Height
15.5 mm, 0.6102 inch
Length of tub
40 mm, 1.5748 inch
Depth
15 mm, 0.5906 inch
Filling volume
13.66 mm, 0.5378 inch