W boat set NO09100-10-4015
- Plansee Material Number
- 11473891
- Plansee Material Number
- 11473891
- Material
- W
- Thickness
- 0.1 mm, 0.0039 inch
- Width
- 9 mm, 0.3543 inch
- Length
- 100 mm, 3.937 inch
- Height
- 3 mm, 0.1181 inch
- Length of tub
- 40 mm, 1.5748 inch
- Depth
- 1.5 mm, 0.0591 inch
- Filling volume
- 0.25 mm, 0.0098 inch
No documents available for this product.