W boat SF08100-30-4017
- Plansee Material Number
- 11490973
- Plansee Material Number
- 11490973
- Material
- W
- Thickness
- 0.3 mm, 0.0118 inch
- Width
- 8 mm, 0.315 inch
- Length
- 100 mm, 3.937 inch
- Height
- 1.7 mm, 0.0669 inch
- Length of tub
- 40 mm, 1.5748 inch
- Depth
- 1.7 mm, 0.0669 inch
- Filling volume
- 0.26 mm, 0.0102 inch
No documents available for this product.