W boat TS14090-10-1020
- Plansee Material Number
- 11518049
- Plansee Material Number
- 11518049
- Material
- W
- Thickness
- 0.1 mm, 0.0039 inch
- Width
- 14 mm, 0.5512 inch
- Length
- 90 mm, 3.5433 inch
- Height
- 5 mm, 0.1969 inch
- Length of tub
- 10 mm, 0.3937 inch
- Depth
- 2 mm, 0.0787 inch
- Filling volume
- 0.08 mm, 0.0031 inch