Mo rod Ø 63,5 mm, cleaned
Contact
Mo Rod Ø 2.5", cleaned
Expand image
Plansee Material Number
12522841
Quantity
Inch
Add to cart
Request for quote
Specifications
Plansee Material Number
12522841
Material
MO
Diameter
63.5 mm, 2.5 inch
Length
0 mm, 0 inch
Documents
Specification
PDF · 284 KB