TaM sheet .039" x 19.685" x 39.370"
- Plansee Material Number
- 164268
- Plansee Material Number
- 164268
- Material
- TAM
- Thickness
- 1 mm, 0.0394 inch
- Width
- 500 mm, 19.685 inch
- Length
- 1000 mm, 39.3701 inch
- Rolled width
- 0 mm, 0 inch
- Rolled length
- 0 mm, 0 inch
- Thickness tolerance +
- 0.08 mm, 0.0031 inch
- Thickness tolerance –
- 0.08 mm, 0.0031 inch