TaM sheet .019" x 19.685" x 39.370"

undefined
Plansee Material Number
256086
PCE
Plansee Material Number
256086
Material
TAM
Thickness
0.5 mm, 0.0197 inch
Width
500 mm, 19.685 inch
Length
1000 mm, 39.3701 inch
Rolled width
0 mm, 0 inch
Rolled length
0 mm, 0 inch
Thickness tolerance +
0.05 mm, 0.002 inch
Thickness tolerance –
0.05 mm, 0.002 inch