Mo sheet .011" x 7.874" x 23.622"

undefined
Plansee Material Number
257467
PCE
Plansee Material Number
257467
Material
MO
Thickness
0.3 mm, 0.0118 inch
Width
200 mm, 7.874 inch
Length
600 mm, 23.622 inch
Rolled width
0 mm, 0 inch
Rolled length
0 mm, 0 inch
Thickness tolerance +
0.02 mm, 8.0E-4 inch
Thickness tolerance –
0.02 mm, 8.0E-4 inch