TaM sheet .009" x 11.811" x 39.370"

undefined
Plansee Material Number
283056
PCE
Plansee Material Number
283056
Material
TAM
Thickness
0.25 mm, 0.0098 inch
Width
300 mm, 11.811 inch
Length
1000 mm, 39.3701 inch
Rolled width
0 mm, 0 inch
Rolled length
0 mm, 0 inch
Thickness tolerance +
0 mm, 0 inch
Thickness tolerance –
0 mm, 0 inch