W rod Ø 3,175 mm, ground
Contact
W Rod Ø 0.125", ground
Expand image
Plansee Material Number
6682
Quantity
Inch
Add to cart
Request for quote
Specifications
Plansee Material Number
6682
Material
W
Diameter
3.175 mm, 0.125 inch
Length
0 mm, 0 inch