Mo boat TS14090-20-1020
- Plansee Material Number
- 11384139
- Plansee Material Number
- 11384139
- Material
- MO
- Thickness
- 0.2 mm, 0.0079 inch
- Width
- 14 mm, 0.5512 inch
- Length
- 90 mm, 3.5433 inch
- Height
- 5 mm, 0.1969 inch
- Length of tub
- 10 mm, 0.3937 inch
- Depth
- 2 mm, 0.0787 inch
- Filling volume
- 0.07 mm, 0.0028 inch