W sheet 0,1 x 200 x 1000 mm
- Plansee Material Number
- 11551986
- Plansee Material Number
- 11551986
- Material
- W
- Thickness
- 0.1 mm, 0.0039 inch
- Width
- 200 mm, 7.874 inch
- Length
- 1000 mm, 39.3701 inch
- Rolled width
- 0 mm, 0 inch
- Rolled length
- 0 mm, 0 inch
- Thickness tolerance +
- 0 mm, 0 inch
- Thickness tolerance –
- 0 mm, 0 inch