W Sheet 0,127 x 508 x 838,2 mm
- Plansee Material Number
- 15267453
- Plansee Material Number
- 15267453
- Material
- W
- Thickness
- 0.127 mm, 0.005 inch
- Width
- 508 mm, 20 inch
- Length
- 838.2 mm, 33 inch
- Rolled width
- 0 mm, 0 inch
- Rolled length
- 0 mm, 0 inch
- Thickness tolerance +
- 0 mm, 0 inch
- Thickness tolerance –
- 0 mm, 0 inch